FIELD: machine building.
SUBSTANCE: procedure for production of refractory ceramic material on base of zirconium consists in zirconium crumbling, in work pieces moulding and in sintering at 1600°C. Zirconium is crumbled in water solution of surface active substance of 0.3-0.5 wt % concentration during 4-10 hours. Polyvinyl alcohol is used as surface active substance.
EFFECT: increased density of items.
2 cl, 2 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
ZIRCON BASED MIXTURE FOR MAKING COMPACT REFRACTORY CERAMICS | 2009 |
|
RU2394004C1 |
ZIRCON-BASED REFRACTORY MATERIAL | 2010 |
|
RU2440952C1 |
METHOD OF PRODUCING OF HEAT RESISTANT ZIRCON-CONTAINING MATERIAL | 2009 |
|
RU2400451C1 |
CHARGE FOR RECEIVING OF REFRACTORY MATERIAL WITH REDUCED HEAD CONDUCTION | 2008 |
|
RU2382016C1 |
METHOD OF PRODUCTION OF FILTERING ARTICLES FROM SILICON DIOXIDE | 2004 |
|
RU2255792C1 |
METHOD OF BLACK CERAMIC PREPARING | 1991 |
|
RU2044717C1 |
METHOD FOR PRODUCTION OF REFRACTORY PARTS | 2003 |
|
RU2245864C1 |
METHOD OF MANUFACTURING CHROMO-ALUMINO-ZIRCONIUM REFRACTORY MATERIALS | 2001 |
|
RU2196118C2 |
PROCESS OF RECEIVING COMPOSITION CERAMIC POWDER ON THE BASIS OF SILICON NITRIDE AND ZIRCONIUM OXIDE AND CHARGE FOR ITS IMPLEMENTATION | 2007 |
|
RU2351435C1 |
METHOD OF PRODUCING SINGLE-PHASE ZIRCON | 2023 |
|
RU2819814C1 |
Authors
Dates
2010-09-20—Published
2009-05-18—Filed