FIELD: metallurgy.
SUBSTANCE: proposed method washing off of regeneration cryolite pulp in condensate formed in heating of cryolite in pulping reactor. Duration of washing-off makes 30-60 minutes, temperature of condensate used for purifying if regeneration cryolite of sulfur compounds makes 50-80°C, volume ratio of used condensate to purifying pump makes (5÷8):1.
EFFECT: reduced costs, high quality.
4 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING GAS CLEANING SLURRY AND DUST PRODUCED IN ALUMINIUM ELECTROWINNING | 2009 |
|
RU2419688C2 |
METHOD OF REFINING REGENERATION CRYOLITE TO REMOVE SODIUM SULFATE | 2004 |
|
RU2274606C2 |
METHOD FOR TREATMENT OF REGENERATION CRYOLITE FROM SODIUM SULFATE | 2001 |
|
RU2217377C2 |
ELECTROLYSIS UNIT FOR ALUMINIUM MANUFACTURE | 2010 |
|
RU2457285C1 |
PROCEDURE FOR PROCESSING SALT SLAG (SLAKED LIME) FORMED AT ALUMINIUM PRODUCING ELECTROLYSER SHUT DOWN FOR REPAIR | 2009 |
|
RU2425179C2 |
METHOD OF PREPARATION TO THE START OF ALUMINIUM CELL | 2006 |
|
RU2324007C2 |
METHOD FOR OBTAINING CRYSTALLINE SODIUM SULFATE FROM LIQUID WASTE OF ELECTROLYTIC ALUMINUM PRODUCTION | 2020 |
|
RU2758438C1 |
ALUMINIUM PRODUCTION SLUDGE DISPOSAL METHOD | 2016 |
|
RU2620844C1 |
METHOD FOR PULP CLEANING FROM TOXIC IMPURITIES SUCH AS CYANIDES, THIOCYANATES, HEAVY METALS, ORGANIC AND INORGANIC COMPOUNDS | 2016 |
|
RU2676979C2 |
METHOD OF PRODUCING MAGNESIUM SULPHATE FROM MAGNESIUM-CONTAINING RAW MATERIAL | 2019 |
|
RU2727382C1 |
Authors
Dates
2010-10-10—Published
2009-05-04—Filed