FIELD: mining industry.
SUBSTANCE: method comprises charging cryolite in rinsing water, washing it at stirring, and dehydration of washed product. Washing is continued until content of sodium sulfate achieves 45-65% that in initial cryolite, which requires time from 5 to 60 min at rinsing water temperature 25 to 70°C and water-to-cryolite weight ratio (3-10):1.
EFFECT: reduced mechanical loss of cryolite due to lesser degree of particle grinding at maximum possible degree of sodium sulfate removal.
4 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR TREATMENT OF REGENERATION CRYOLITE FROM SODIUM SULFATE | 2001 |
|
RU2217377C2 |
METHOD OF PRODUCING ALKALI-FREE MINERALIZER FOR BURNING CLINKER FROM FLUORINE-CONTAINING WASTES OF ALUMINIUM PRODUCTION | 2023 |
|
RU2821274C1 |
METHOD OF PROCESSING FLUOROCARBON-CONTAINING WASTES OF ELECTROLYTIC ALUMINUM PRODUCTION | 2003 |
|
RU2247160C1 |
ALUMINIUM PRODUCTION SLUDGE DISPOSAL METHOD | 2016 |
|
RU2620844C1 |
METHOD OF PROCESSING OF SODIUM-FLUORINE-CARBON-CONTAINING WASTE OF ELECTROLYTIC PRODUCTION OF ALUMINIUM | 2016 |
|
RU2624570C1 |
METHOD OF PRODUCING ALUMINIUM FLUORIDE | 2011 |
|
RU2462418C1 |
METHOD OF TREATMENT OF THE REGENERATION CRYOLITE | 2017 |
|
RU2667447C1 |
METHOD OF PREPARING CRYOLITE | 1997 |
|
RU2140396C1 |
METHOD OF PRODUCING COMPLEX ADDITIVE FOR SINTERING PORTLAND CEMENT CLINKER | 2023 |
|
RU2814678C1 |
METHOD OF EXTRACTING RARE-EARTH METALS (REM) FROM PHOSPHOGYPSUM | 2012 |
|
RU2492255C1 |
Authors
Dates
2006-04-20—Published
2004-05-25—Filed