FIELD: metallurgy.
SUBSTANCE: alloy on base of aluminium contains following components wt %: zinc 5-8, magnesium 2-3.1, nickel 1-4.2, iron 0.02-1, zirconium 0.02-0.25 %, copper 0.05-0.3 %. Also, temperature of equilibrium solidus of material is as high as 550°C and hardness is as high as 180 HV. Alloy has a structure corresponding to matrix formed with solid solution of aluminium with uniformly distributed disperse particles of secondary discharges in it and particles of aluminides containing nickel and iron of eutectic origin uniformly distributed in matrix. Also, alloy contains matrix and aluminides at the following ratio, vol % aluminides containing nickel and iron 5.0-6.3, matrix - the rest.
EFFECT: production of new high-strength alloy thermally hardenable and designed both for fabrication of shaped casting and of deformed semi-products.
4 cl, 5 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
HIGH-STRENGTH SPARINGLY-ALLOYED ALUMINIUM-BASED ALLOY | 2012 |
|
RU2484168C1 |
HIGH-STRENGTH ALLOY BASED ON ALUMINIUM WITH CALCIUM ADDITION | 2012 |
|
RU2478132C1 |
ALUMINUM-BASED MATERIAL | 2003 |
|
RU2245388C1 |
ALUMINUM-BASE MATERIAL | 2005 |
|
RU2288965C1 |
HIGH-STRENGTH FOUNDRY ALUMINUM ALLOY WITH CALCIUM ADDITIVE | 2019 |
|
RU2713526C1 |
HIGH-STRENGTH FOUNDRY ALUMINUM ALLOY WITH CALCIUM ADDITIVE | 2018 |
|
RU2691476C1 |
CASTABLE ALUMINIUM ALLOY | 2008 |
|
RU2405852C2 |
METHOD FOR PRODUCING CASTINGS OF HIGH-STRENGTH ALUMINIUM-BASED ALLOYS | 2015 |
|
RU2621499C2 |
CAST ALUMINIUM ALLOY-(SPARINGLY-ALLOYED HIGH-STRENGTH SILUMIN) | 2010 |
|
RU2441091C2 |
CASTING ALUMINIUM ALLOY | 2011 |
|
RU2485199C1 |
Authors
Dates
2011-05-27—Published
2009-08-07—Filed