FIELD: metallurgy.
SUBSTANCE: alloy contains the following, wt %: silicon 6.6-7.4, magnesium 0.31-0.45, copper 0.18-0.32, manganese 0.15-0.45, iron 0.15-0.4, aluminium is the rest, at that, the alloy has liquidus temperature within 608 to 620°C; temperature of balanced solidus of not less than 552°C and structure after heat treatment as per mode T66, which contains the amount of inclusions of silicon phase within 6.4 to 7.5 vol. %; iron in the alloy structure is completely bound to skeletal inclusions of phase Al15(Fe,Mn)3Si2, and magnesium is completely bound to secondary extractions of phase Al15Cu2Mg8Si6.
EFFECT: creation of alloy for obtaining high-duty shaped castings and having high technological and operating characteristics.
2 cl, 2 tbl, 2 ex, 2 dwg
Title | Year | Author | Number |
---|---|---|---|
CAST ALUMINIUM ALLOY-(SPARINGLY-ALLOYED HIGH-STRENGTH SILUMIN) | 2010 |
|
RU2441091C2 |
CASTABLE ALUMINIUM ALLOY | 2008 |
|
RU2405852C2 |
CAST ALLOY ON BASE OF ALUMINIUM | 2009 |
|
RU2415193C1 |
HIGH-STRENGTH CAST ALUMINUM ALLOY | 2020 |
|
RU2754418C1 |
CASTING ALUMINUM-SILICON ALLOY | 2017 |
|
RU2659514C1 |
CASTABLE MAGNESIUM ALLOY | 2012 |
|
RU2506337C1 |
ALUMINIUM ALLOY | 2016 |
|
RU2647070C2 |
HIGH-STRENGTH SPARINGLY-ALLOYED ALUMINIUM-BASED ALLOY | 2012 |
|
RU2484168C1 |
ALUMINIUM-MATRIX COMPOSITE MATERIAL WITH BORON-CONTAINING FILLER | 2012 |
|
RU2496902C1 |
HEAT-RESISTANT ALUMINIUM-BASED ALLOY AND METHOD FOR OBTAINING DEFORMED SEMI-FINISHED PRODUCTS FROM IT | 2010 |
|
RU2446222C1 |
Authors
Dates
2013-06-20—Published
2011-12-02—Filed