FIELD: chemistry.
SUBSTANCE: method involves saturating fibre with an alcohol solution or aqueous emulsion containing 0.5-10.5% oligo(3-aminopropyl)(octyl)ethoxysiloxane, drying in air and forming a nonwoven web followed by needling. Thermal treatment at 100-140°C for 5-10 minutes is carried out in order to hold the oligo(3-aminopropyl)(octyl)ethoxysiloxane on the surface of the fibre.
EFFECT: nonwoven material has high strength, sorption capacity, water absorption and soaking capacity.
5 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR PRODUCING OF NON-WOVEN TEXTILE HIGH-STRENGTH MATERIALS | 2006 | 
 | RU2300585C1 | 
| METHOD FOR MANUFACTURE OF NONWOVEN NEEDLE-PUNCHING MATERIAL REINFORCED WITH MESH | 2007 | 
 | RU2360050C2 | 
| NEEDLE-PUNCHED FABRIC AND METHOD OF ITS PRODUCTION | 2007 | 
 | RU2365687C1 | 
| PRODUCTION OF NONWOVEN MATERIAL FROM POLYESTER FIBRES | 2024 | 
 | RU2837477C1 | 
| METHOD FOR MAKING NONWOVEN NEEDLED FELT | 2007 | 
 | RU2345183C1 | 
| NONWOVEN FILTERING MATERIAL | 0 | 
 | SU1346199A1 | 
| NONWOVEN MATERIAL | 2002 | 
 | RU2208074C1 | 
| NONWOVEN MATERIAL | 2015 | 
 | RU2594455C1 | 
| NONWOVEN FILTERING MATERIAL FOR RECLAMATION | 0 | 
 | SU1320294A1 | 
| NONWOVEN MATERIAL | 2015 | 
 | RU2593142C1 | 
Authors
Dates
2011-10-20—Published
2010-04-20—Filed