FIELD: process engineering.
SUBSTANCE: invention relates to metallurgy and may be used in slag-pot transfer car repair. Bores are drilling one crack edges and crack welding groove is performed. Crack is welded in several layers by semiautomatic welding machine at 350-500 A with welded bead joint downed relative of welding groove edges. Build-up metal is upset-forged layer by layer. Zone of fusion between welded bead joint and main metal is upset-forged to remove back side of root seam to be, then, penetrated.
EFFECT: lower labor input, higher quality.
2 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
CASTINGS REPAIRE METHOD, USING THE ARC WELDING | 2015 |
|
RU2630080C2 |
METHOD OF ELECTRIC-ARC WELDING | 1997 |
|
RU2110378C1 |
METHOD OF REPAIRING DEFECTS OF CASTING | 0 |
|
SU1555099A1 |
REPAIR METHOD OF CRACKS OF METALLIC STRUCTURES | 2008 |
|
RU2378098C1 |
METHOD OF REPAIRING FRACTURES IN METAL STRUCTURES | 2011 |
|
RU2466843C1 |
HIGH-STRENGTH STEEL WELDING METHOD | 1988 |
|
RU2103128C1 |
METHOD OF REPAIRING FRACTURES IN METAL STRUCTURES | 2010 |
|
RU2444425C2 |
METHOD FOR INDERECT WELDING OF DN 800 PIPE OF MULTIPLE FORCED CIRCULATION LOOP OF POWER UNITS WITH RBMK-1000 REACTOR PLANT | 2021 |
|
RU2759272C1 |
METHOD OF REPAIR OF CRACKS | 0 |
|
SU1593876A1 |
METHOD OF ARC WELDING OF WELDOLET FROM AUSTENITE STEELS TO PIPELINE FROM LOW-CARBON AND LOW-ALLOY STEELS | 2016 |
|
RU2643098C2 |
Authors
Dates
2012-01-10—Published
2010-11-01—Filed