FIELD: machine-building industry.
SUBSTANCE: compound contains (wt %): ε-caprolaktam - 97-98, metal sodium metal - 0.07, toluylene diisocyanate - 0.257 and a mixture of merkupral and dithizone at a ratio 10:1 - 0.29-0.98. Friction factor 0.08-0.12, wear 0.006-0.002, water absorption 0.20 % during 20 days.
EFFECT: improved physical and mechanical properties of compound.
1 tbl, 4 ex
| Title | Year | Author | Number |
|---|---|---|---|
| ANTI-FRICTIONAL SELF-LUBRICATING COMPOSITE MATERIAL OF THE "MASLYANIT" [OILANITE] GROUP | 2020 |
|
RU2743134C1 |
| METHOD FOR PRODUCING POLYAMIDE-BASED COMPOSITE MATERIAL | 2017 |
|
RU2661235C1 |
| POLYAMIDE COMPOSITE MATERIAL (VARIANTS) | 2006 |
|
RU2316571C1 |
| METHOD OF OBTAINING POLYCAPROAMIDE | 0 |
|
SU1147722A1 |
| POLYAMIDE COMPOSITION AND METHOD FOR PREPARATION THEREOF | 2011 |
|
RU2488613C2 |
| ADHESION ACTIVATING AGENT OF RUBBERS TO BRASS-COATED METAL | 2007 |
|
RU2380385C2 |
| ANTIFRICTION WOOD-POLYMER MATERIAL | 2008 |
|
RU2383570C2 |
| POLYAMIDE COMPOSITE MATERIAL (VERSIONS) | 2009 |
|
RU2416623C2 |
| METHOD OF FABRICATING "CAPROLONE" PRODUCTS | 1994 |
|
RU2090363C1 |
| ANTIFRICTION COMPOSITION | 0 |
|
SU1479474A1 |
Authors
Dates
2012-01-10—Published
2010-07-15—Filed