FIELD: metallurgy.
SUBSTANCE: proposed method consists in valuable metals are decomposed in salt melt containing 60-95 wt % of NaOH and 5-40 wt % of Na2SO4. Then, melt decomposition product is converted into solid phase by cooling to room temperature. After cooling, minced melt decomposition product is converted in water at temperature lower than 80°C to produce water suspension and water fraction is separated by filtration for components to be extracted therefrom.
EFFECT: higher efficiency of extraction.
22 cl, 1 dwg, 3 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| VALUABLE METAL EXTRACTION PROCESS FROM SUPER-ALLOYS | 2002 |
|
RU2313589C2 |
| PRODUCTION OF VALVE METAL POWDERS | 2004 |
|
RU2362653C2 |
| METHOD FOR PRODUCING CHARGE | 2016 |
|
RU2638195C1 |
| TANTALUM-BASE ALLOY REFINING METHOD | 2012 |
|
RU2499065C1 |
| NICKEL-BASED SUPERALLOY, SINGLE CRYSTAL BLADE AND GAS TURBINE ENGINE | 2017 |
|
RU2749981C2 |
| METHOD OF THERMOCHEMICAL PROCESSING OF RARE METAL RAW MATERIAL | 2014 |
|
RU2592655C2 |
| METHOD OF EXTRACTING NOBLE METALS FROM WASTES | 1988 |
|
SU1840855A1 |
| METHOD OF FABRICATION OF TANTALUM OR NIOBIUM POWDER | 2008 |
|
RU2384390C1 |
| RECLAMATION OF BARRIER METAL POWDERS | 2005 |
|
RU2404881C2 |
| PROCESSING WASTES CONTAINING NONFERROUS AND PLATINUM METALS | 2012 |
|
RU2484154C1 |
Authors
Dates
2012-04-10—Published
2007-06-29—Filed