FIELD: chemistry.
SUBSTANCE: method involves applying a protective coating onto an ethynol film. The protective coating used is a composition which is latex SKS-65 with filler in form of aluminium powder in amount of 1 ppm latex SKS-65 and 0.15 ppm aluminium powder.
EFFECT: improved light-reflecting properties of coating films made from ethynol varnish, as well as high weather resistance and longevity.
1 ex
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PROTECTING POLYMER MATERIALS FROM ULTRAVIOLET RADIATION | 2011 |
|
RU2471838C1 |
| ETHYNOL PERLITE CONCRETE | 2012 |
|
RU2519249C2 |
| AGGLOPORITE CONCRETE | 2010 |
|
RU2459783C2 |
| METHOD OF GLUING ROLL MATERIALS | 2015 |
|
RU2580863C1 |
| METHOD OF ACCELERATING HARDENING OF ETHYNOL VARNISH-BASED POLYMER COATINGS | 2010 |
|
RU2455327C1 |
| METHOD OF GLUING SURFACES | 2011 |
|
RU2462495C1 |
| PROTECTIVE COMPOSITION FOR WOODEN BUILDING STRUCTURES | 2013 |
|
RU2534795C1 |
| EXPANDED-CLAY CONCRETE STRUCTURAL MATERIAL | 2010 |
|
RU2459782C2 |
| PROTECTIVE-MECHANICAL COATING OF MONOLITHIC HEAT INSULATION | 2010 |
|
RU2454597C1 |
| METHOD OF ACCELERATING SOLIDIFICATION OF POLYMER COATINGS BASED ON ETHYNOL VARNISH | 2013 |
|
RU2540306C1 |
Authors
Dates
2012-04-20—Published
2010-11-26—Filed