FIELD: metallurgy.
SUBSTANCE: steel contains the following, wt %: carbon 0.03-0.06, silicon 0.10-0.60, manganese 0.80-2.00, chrome 22.00-24.00, nickel 14.00-16.00, molybdenum 0.80-1.50, copper 0.80-1.50, vanadium 0.08-0.15, niobium 0.02-0.12, nitrogen 0.45-0.55, zirconium 0.02-0.040, cerium 0.005-0.02, calcium 0.005-0.02, aluminium 0.005-0.02, iron and impurities are the rest.
EFFECT: steel has high mechanical properties and high resistance to pit and crevice corrosion at maintaining non-magnetic level.
2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
HIGH-NITROGEN NONMAGNETIC CORROSION-RESISTANT STEEL | 2011 |
|
RU2451765C1 |
HIGH-STRENGTH NONMAGNETIC RUSTPROOF CASTING STEEL AND METHOD OF ITS THERMAL TREATMENT | 2010 |
|
RU2447185C1 |
HIGH-STRENGTH NONMAGNETIC CORROSION-RESISTANT STEEL | 2018 |
|
RU2683173C1 |
HEAT-RESISTANT STEEL FOR WATER-COOLED MOLDS | 2012 |
|
RU2494167C1 |
AUSTENITIC-FERRITIC STAINLESS STEEL | 2019 |
|
RU2700440C1 |
MARTENSITE STEEL FOR CRYOGENIC EQUIPMENT | 2015 |
|
RU2594572C1 |
CASTING OF HIGH-STRENGTH WEAR-RESISTANT STEEL AND METHODS FOR HEAT TREATMENT OF CASTINGS OF HIGH-STRENGTH WEAR-RESISTANT STEEL | 2020 |
|
RU2753397C1 |
THICK COLD-RESISTANT STEEL | 2017 |
|
RU2665854C1 |
CORROSION-RESISTANT HIGH-STRENGTH NON-MAGNETIC STEEL | 2019 |
|
RU2696792C1 |
HEAT-RESISTANT STEEL | 2011 |
|
RU2441092C1 |
Authors
Dates
2012-06-27—Published
2011-05-31—Filed