FIELD: metallurgy.
SUBSTANCE: normalisation is performed at temperature of 960°-970°C during 30-50 minutes, cooling is performed in the air, drawing is performed at 760°-770°C with exposure at that temperature during 60-80 minutes, and cooling is performed to 680°C with furnace during 50-70 minutes with final cooling in the air.
EFFECT: providing stability of yield strength values, which will allow improving the quality of pipes and operating reliability and lifetime of steam generator; performing the heat treatment including pipe normalisation and drawing operations.
6 ex, 1 tbl, 3 dwg
Title | Year | Author | Number |
---|---|---|---|
COLD DEFORMED PIPE MANUFACTURING METHOD | 2011 |
|
RU2464325C1 |
METHOD FOR PRODUCTION OF SEAMLESS COLD-DEFORMED HIGH-STRENGTH PIPES FROM ALLOY UNS N06625 | 2020 |
|
RU2732818C1 |
THERMAL TREATMENT OF CASTS FROM RUSTPROOF MARTENSITE STEEL | 2013 |
|
RU2526107C1 |
HUB WITH FLANGE RESTORATION METHOD | 1997 |
|
RU2115532C1 |
METHOD OF FABRICATING THIN-WALLED PIPES | 2008 |
|
RU2391162C2 |
METHOD OF PRODUCTION OF PRECISION PIPES | 2006 |
|
RU2330739C2 |
METHOD OF AGEING OF HEAT RESISTANT ALLOYS | 2005 |
|
RU2366725C2 |
STRUCTURE STEEL OF HIGH IMPACT RESILIENCE AT CRYOGENIC TEMPERATURE | 2009 |
|
RU2414520C1 |
MANUFACTURING METHOD OF ROLLED SECTION IN BUNDLES AND FACILITY FOR ITS IMPLEMENTATION | 2008 |
|
RU2368436C9 |
HETEROGENEOUS STEEL WELDING METHOD | 1991 |
|
RU2022738C1 |
Authors
Dates
2012-10-20—Published
2011-07-19—Filed