FIELD: metallurgy.
SUBSTANCE: Anhydrous gadolinium trichloride is used as gadolinium source, potassium fluoroborate is used as boron source, and equimolar mixture of potassium and sodium chlorides is used as base electrolyte. Electrolysis is carried out in potentiostatic mode at temperature of 700±10°C, current densities of - 0.1 to - 1.0 A/cm2 and electrolysis potential of - 2.6 to -2.8 V relative to glass-carbon quasi-stationary comparison electrode.
EFFECT: obtaining pure ultrafine powder of gadolinium hexaboride; increase in synthesis rate of target product from molten electrolyte and reduction of costs.
2 cl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTIC METHOD OF PRODUCING ULTRAFINE GADOLINIUM HEXABORIDE POWDER | 2012 |
|
RU2507314C1 |
ELECTROLYTIC METHOD FOR OBTAINING ULTRADISPERSE POWDER OF LANTHANUM HEXABORIDE | 2011 |
|
RU2477340C2 |
ELECTROLYTIC METHOD FOR OBTAINING ULTRAFINE POWDER OF DYSPROSIUM HEXABORIDE | 2012 |
|
RU2510630C1 |
ELECTROLYTIC METHOD OF OBTAINING NANOSIZED CERIUM HEXABORIDE POWDER | 2013 |
|
RU2540277C1 |
ELECTROLYTIC METHOD OF OBTAINING NANOSIZED POWDER OF NEODYMIUM HEXOBORIDE | 2008 |
|
RU2389684C2 |
ELECTROLYTIC METHOD OF PRODUCING ULTRAFINE CERIUM HEXABORIDE POWDER | 2011 |
|
RU2466090C1 |
ELECTROLYTIC METHOD FOR SYNTHESIS OF PRASEODYMIUM HEXABORIDE | 2008 |
|
RU2393115C2 |
ELECTROLYTIC METHOD OF PRODUCING SUPERDISPERSED POWDER OF CERIUM AND COBALT BORIDE | 2018 |
|
RU2695346C1 |
ELECTROCHEMICAL METHOD OF PRODUCING MICRODISPERSE POWDERS OF METAL HEXABORIDES OF LANTHANIDE GROUP | 2019 |
|
RU2722753C1 |
METHOD OF PRODUCING NANODISPERSED YTTRIUM HEXABORIDE POWDER | 2009 |
|
RU2448044C2 |
Authors
Dates
2012-11-10—Published
2011-05-18—Filed