FIELD: chemistry.
SUBSTANCE: composition contains the following (pts.wt): epoxide oligomer 29-35, oligoamidoamide 4-7, hollow glass microspheres 25-33, ammonium phosphate 15-21.5, aliphatic amine 8-12, catalyst 0.5-1, rubber 3-6 and powdered filler 2.5-3.5.
EFFECT: invention enables to obtain a polymer composition which solidifies in 6-12 hours at room temperature and has high compression strength and impact viscosity.
7 cl, 3 tbl, 3 ex
| Title | Year | Author | Number |
|---|---|---|---|
| POLYMER COMPOSITION | 2013 |
|
RU2540084C1 |
| POLYMER COMPOSITION, METHOD FOR ITS PREPARATION AND POLYMERIZATION | 2023 |
|
RU2818758C1 |
| EPOXIDE COMPOSITION | 2016 |
|
RU2618557C1 |
| REPAIR COMPOSITION | 2014 |
|
RU2573518C1 |
| SELF-DAMPING POLYMERIC COMPOSITION | 2002 |
|
RU2220990C2 |
| COMPOSITION FOR PRODUCING A FIRE-RESISTANT ANTI-CORROSIVE HEAT INSULATION COATING AND METHOD FOR THE PRODUCTION THEREOF (VARIANTS) | 2021 |
|
RU2779120C1 |
| EPOXIDE GLUE COMPOSITION | 2007 |
|
RU2368636C2 |
| HEAT-RESISTANT FOAMED POLYMER COMPOSITE MATERIAL, METHOD OF PRODUCING BASE THEREFOR AND METHOD OF PRODUCING MATERIAL | 2013 |
|
RU2545287C1 |
| THERMOSTABLE COMPOSITIONAL MATERIAL AND METHOD FOR OBTAINING THEREOF | 2014 |
|
RU2573468C2 |
| COMPOSITION FOR HEAT-SHIELDING COATING | 1992 |
|
RU2043378C1 |
Authors
Dates
2013-01-10—Published
2011-07-04—Filed