FIELD: metallurgy.
SUBSTANCE: proposed method comprises loading charge composed of the mix of steel and iron chips into alundum crucible, smelting in furnace at 1250-1300°C, holding at said temperature for 3-4 min, unloading from the furnace and tempering in water to produce a ledeburite form inhomogeneity composed of white pig iron. Then, obtained ingot is heated to 680-800°C, forged and tempered to obtain composite structure martensite-white pig iron.
EFFECT: simplified process, homogeneous properties.
1 tbl, 8 dwg, 1 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR OBTAINING PORE-FREE CARBIDE CAST IRON FOR MANUFACTURE OF PLANISHING MACHINES | 2012 | 
 | RU2511226C2 | 
| METHOD OF MAKING DAMASK STEEL | 1992 | 
 | RU2051184C1 | 
| METHOD FOR PRODUCING MILLING BALLS FROM WHITE ALLOYED CAST IRON | 1999 | 
 | RU2169787C2 | 
| METHOD OF PRODUCTION MULTILAYER STEEL ARTICLES (VERSIONS) | 2007 | 
 | RU2351476C2 | 
| METHOD FOR PRODUCTION OF DAMASCUS STEEL | 1996 | 
 | RU2103380C1 | 
| METHOD OF RECEIVING PRODUCTS MADE OF IRON WITH CARBON ALLOY | 2008 | 
 | RU2352671C1 | 
| METHOD OF PRODUCTION OF INGOTS MADE OUT OF MOTTLED CAST IRON WITH AUSTENITIC-BAINITE STRUCTURE | 2003 | 
 | RU2250268C1 | 
| CAST IRON | 0 | 
 | SU1723180A1 | 
| ALLOYED STEEL | 1998 | 
 | RU2149207C1 | 
| EUTECTIC ALLOY | 0 | 
 | SU1733494A1 | 
Authors
Dates
2013-05-27—Published
2012-03-13—Filed