FIELD: chemistry.
SUBSTANCE: electrolyte contains the following, g/l: zinc sulphate 200-240, iron sulphate 15-20, sodium carbonate 80-120, ammonium sulphate 30, tetraethylammonium hydrochloride 3-4.
EFFECT: high adhesion of the coating to components, electrolyte stability and reduced dendrid formation.
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTE COMPOSITION OF ANTIFRICTION ELECTROLYTIC ZINC-IRON ALLOY FOR DEPOSITION IN HYDROMECHANICAL ACTIVATION CONDITIONS | 2015 |
|
RU2633866C2 |
ELECTROLYTE FOR DEPOSITING ZINC-IRON ALLOY | 1993 |
|
RU2086712C1 |
ELECTROLYTE FOR DEPOSITION OF COAT | 1999 |
|
RU2169799C1 |
CADMIUM-ZINC PLATING DEPOSITION ELECTROLYTE | 2007 |
|
RU2350697C1 |
ELECTROLYTE FOR ELECTRODEPOSITION OF ZINC-IRON COATINGS | 2019 |
|
RU2712582C1 |
ELECTROLYTE FOR ELECTRODEPOSITION OF LUSTROUS ZINC COATINGS | 2024 |
|
RU2820435C1 |
ELECTROLYTE FOR SEDIMENTATION OF ALLOY AURUM-BORON | 2008 |
|
RU2362841C1 |
ELECTROLYTE FOR DEPOSITION OF SILVER-INDIUM ALLOY | 2009 |
|
RU2386731C1 |
ELECTROLYTE FOR COAT DEPOSITION | 2003 |
|
RU2250935C1 |
ELECTROLYTE FOR SEDIMENTATION OF COMPOSITION COATING NICKEL-COBALT-DIAMOND | 2008 |
|
RU2362843C1 |
Authors
Dates
2013-08-10—Published
2011-01-12—Filed