FIELD: electrolytic deposition of hard, wear resistant coats, in particular iron-boron coats useful in surface reducing and hardening.
SUBSTANCE: claimed electrolyte contains (kg/m3): iron (II) chloride 350-400, boric acid 2.5-60; hydrochloric acid 0.5-2.
EFFECT: coats of increased microhardness and wear resistance.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY-BASED COAT | 2003 |
|
RU2250936C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-ALUMINUM ALLOY | 2003 |
|
RU2263727C2 |
METHOD OF ELECTROLYTIC DEPOSITION OF AN IRON-TITANIUM ALLOY | 2003 |
|
RU2230139C1 |
ELECTROLYTIC DEPOSITION METHOD OF IRON COATING | 2023 |
|
RU2816237C1 |
METHOD OF ELECTROLYTIC PRECIPITATION OF IRON-MOLYBDENUM DISULFIDE COATING | 2013 |
|
RU2537686C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-TUNGSTEN ALLOY | 2001 |
|
RU2192509C2 |
METHOD OF ELECTRODEPOSITION OF FERROMOLYBDENUM ALLOY | 2000 |
|
RU2174163C1 |
ELECTROLYTE FOR DEPOSITION OF COAT | 1999 |
|
RU2169799C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2015 |
|
RU2634555C2 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2002 |
|
RU2230836C1 |
Authors
Dates
2005-04-27—Published
2003-09-19—Filed