FIELD: textiles, paper.
SUBSTANCE: method of production of cellulose lies in cooking wood chips at a temperature of 90-98°C, thorough mixing and at atmospheric pressure of 740-760 mm Hg in a mixture containing 3.9-5.6 wt % hydrogen peroxide, 25.2-26.7 wt % acetic acid in the presence of 2.0 % by weight of sulfuric acid catalyst chips with a duration of cooking of 2.5-3.5 hours, and irrigation modulus of 5-10 with subsequent isolation of the target product.
EFFECT: simplifying the method of production of cellulose, increase in target product yield, improvement of quality characteristics of the target product by increasing the content in it of holocellulose and reduction of residual lignin.
1 tbl, 11 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CELLULOSE OBTAINING | 2013 |
|
RU2547689C1 |
METHOD OF COMPLEX PROCESSING OF BIRCH WOOD | 2016 |
|
RU2620551C1 |
METHOD FOR PRODUCING FIBROUS SEMI-FINISHED PRODUCT | 2023 |
|
RU2807731C1 |
METHOD OF PRODUCING CELLULOSE | 2015 |
|
RU2590882C1 |
METHOD FOR PRODUCING OF CELLULOSE SEMI-FINISHED PRODUCT FROM LARCH WOOD | 2004 |
|
RU2251602C1 |
METHOD OF PRODUCING CELLULOSE FOR CHEMICAL PROCESSING | 2020 |
|
RU2738813C1 |
METHOD OF PREPARING CELLULOSE HALF-FINISHED PRODUCT | 2001 |
|
RU2181807C1 |
METHOD OF PREPARING CELLULOSE INTERMEDIATE | 1999 |
|
RU2150538C1 |
METHOD OF PRODUCING PULP | 0 |
|
SU1721152A1 |
METHOD OF PRODUCING CELLULOSE STOCK FROM HARDWOOD | 1992 |
|
RU2092641C1 |
Authors
Dates
2013-08-20—Published
2012-03-23—Filed