FIELD: chemistry.
SUBSTANCE: method of obtaining cellulose consists in cooking wood chips at a temperature of 98-100°C, intensive mixing and atmospheric pressure in a mixture, which contains 3.0-5.6 wt % of hydrogen peroxide and 15.0-25.0 wt % of acetic acid in the presence of a titanium dioxide catalyst, present in an amount of 0.5-1.0% of the chips weight with cooking duration for 2.5-3.5 hours and a hydromodulus of 5-15 with the following separation of the target product.
EFFECT: improvement of the ecological safety of the process and simplification of the method due to the application of the inert titanium dioxide catalyst with the preservation of high output and quality of the cellulose product.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING CELLULOSE | 2015 |
|
RU2590882C1 |
METHOD OF PRODUCTION OF CELLULOSE | 2012 |
|
RU2490384C1 |
METHOD OF COMPLEX PROCESSING OF BIRCH WOOD | 2016 |
|
RU2620551C1 |
METHOD OF PREPARING CELLULOSE HALF-FINISHED PRODUCT | 2001 |
|
RU2181807C1 |
METHOD OF PRODUCING CELLULOSE FOR CHEMICAL PROCESSING | 2020 |
|
RU2738813C1 |
METHOD OF PRODUCING CELLULOSE WOOD PULP | 2011 |
|
RU2474635C1 |
METHOD OF CELLULOSE SEMI-FINISHED PRODUCT PRODUCTION | 2003 |
|
RU2217537C1 |
METHOD FOR PRODUCING FIBROUS SEMI-FINISHED PRODUCT | 2023 |
|
RU2807731C1 |
METHOD OF PREPARING CELLULOSE INTERMEDIATE | 1999 |
|
RU2150538C1 |
METHOD FOR PRODUCING OF CELLULOSE SEMI-FINISHED PRODUCT FROM LARCH WOOD | 2004 |
|
RU2251602C1 |
Authors
Dates
2015-04-10—Published
2013-12-10—Filed