FIELD: oil and gas industry.
SUBSTANCE: method includes preparation, pre-heating and tempering of source oil stock, at the same time moist oil stock is exposed to grinding to fraction of 0-25 mm, dried by internal smoke gases with rated speed of 60-90 m/sec and temperature of 350-400°C in the suspended layer with fountain-like circulation of coke particles to 0.5-2% of moisture content, exposed to cyclone separation with provision of trap ratio of more than 97% and with sifting of dust-like particles with fraction from 0 to less than 2 mm, which is treated with greasing agent with consumption of 0.5-1.0 wt %, per 1 one of coke, and stabilised hot coke with T-60-90°C of fraction more than 2-25 mm is tempered in a rotary drum furnace.
EFFECT: invention makes it possible to increase productivity of tempering furnaces, to stabilise process mode of coke tempering, to improve quality of oil coke, to reduce specific power inputs, to produce commercial product, to reduce anthropogenic emissions into environment.
1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CALCINING PITCH COKE | 1998 |
|
RU2128211C1 |
METHOD OF METALLURGICAL COKE PRODUCTION | 2013 |
|
RU2553116C1 |
0 |
|
SU239206A1 | |
METHOD OF OIL COKE CALCINATION | 0 |
|
SU747814A1 |
COAL CHARGE PREPARATION FOR COKING | 2012 |
|
RU2550874C2 |
METHOD OF COKE CALCINING | 0 |
|
SU806746A1 |
METHOD FOR CALCINATING PETROLEUM COKE | 0 |
|
SU1130589A1 |
METHOD OF PREPARING ELECTRODE PASTE | 1997 |
|
RU2132411C1 |
METHOD FOR FORMING FINE FACTIONS OF OIL COKE | 2017 |
|
RU2660129C1 |
PROCESS OF PREPARATION OF ELECTRODE COKE FOR PRODUCTION OF ANODE MASS | 2001 |
|
RU2186882C1 |
Authors
Dates
2013-09-10—Published
2011-12-27—Filed