FIELD: chemistry.
SUBSTANCE: invention can be applied in electronics, solar energy industry, atomic industry, metallurgy. Pitch coke is tempered at 1200-1300 °C during 2-3 hours. Then its vibration grinding is carried out until middle-sized particles in the range 5-20 microns are obtained. Coal pitch is modified by mixing with carbonaceous nano-additive in quantity 0.2-1.2 wt %, heated with mixing to 280-300 °C, cooled to temperature of the environment and crushed to size 2 mm. Coke, pitch with nano-additive and stearic acid are dosed and mixed in mixing machine at 210-270 °C. Obtained mass is cooled to temperature of the environment, crushed by jaw and hammer crushers, milled by vibration mill until press-powder of required coarseness is obtained, with its further pressing on isostatic press. Obtained work pieces are burned, impregnated, re-burnt, graphitised and mechanically processed.
EFFECT: invention makes it possible to obtain products of large size with high physical-chemical characteristics.
5 cl, 5 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURE OF STRUCTURAL GRAPHITE | 2003 |
|
RU2258032C1 |
COMPOSITION AND METHOD FOR PREPARING CHARGE FOR PRODUCTION OF CARBON MATERIAL | 1997 |
|
RU2134656C1 |
EXTRUSION METHOD FOR PRODUCING A PITCH-COKE COMPOSITION FOR MANUFACTURING GRAPHITE MATERIALS BASED ON A FINE-GRAINED FILLER OF AN ISOTROPIC STRUCTURE | 2021 |
|
RU2771657C1 |
METHOD FOR PRODUCTION OF CARBON-CONTAINING MASS FOR PRODUCTION OF GRAPHITIZED ARTICLES | 1993 |
|
RU2051090C1 |
METHOD OF FINE GRAIN GRAPHITE PRODUCTION | 1992 |
|
RU2069205C1 |
FINE-GRAIN GRAPHITE PREPARATION PROCESS | 2004 |
|
RU2257341C1 |
METHOD OF OBTAINING BURNT AND GRAPHITED CARBONE MATERIALS | 2007 |
|
RU2344992C1 |
METHOD OF PRODUCING HIGH-DENSITY GRAPHITE | 2012 |
|
RU2496714C1 |
0 |
|
SU614025A1 | |
ANTIFRICTION SELF-LUBRICATING MATERIAL | 0 |
|
SU1097656A1 |
Authors
Dates
2013-09-20—Published
2012-01-11—Filed