FIELD: electricity.
SUBSTANCE: articles are painted by preparing epoxy enamel EPIMAL®-9114 by adding 30% solution of 2-methylimidazole in diethylene glycol in amount of 0.5-1.0% of the weight of enamel. The enamel is dried for 16-22 minutes at temperature of 180-200°C to obtain a coating.
EFFECT: method improves the quality of coating and provides the required degree of drying.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING COATINGS FOR ELECTRORADIOPRODUCTS | 2012 |
|
RU2516549C2 |
METHOD FOR PAINTING AND DRYING OF RADIO ELEMENTS | 2009 |
|
RU2385513C1 |
EPOXY MARKING COMPOSITION (VERSIONS) | 2017 |
|
RU2644460C1 |
ENAMEL FOR COLOUR CODE MARKING OF ELECTRONIC TECHNOLOGY | 2008 |
|
RU2421491C2 |
POLYESTER ENAMEL | 2005 |
|
RU2287546C1 |
PRIMING ENAMEL FOR PROTECTIVE ANTI-CORROSION EPOXY COATING PROTECTIVE LAYER UP TO 500 MICRONS, METHOD FOR PROTECTIVE ANTI-CORROSION EPOXY COATING FORMATION, AND PRODUCT WITH PROTECTIVE ANTI-CORROSION EPOXY COATING | 2015 |
|
RU2613985C1 |
ANTICORROSION PROTECTION OF METAL STRUCTURES AND LARGE-SIZE INDUSTRIAL EQUIPMENT | 2011 |
|
RU2481365C1 |
NITROCELLULOSE-POLYURETHANE PAINT-VEHICLE COMPOSITION | 1996 |
|
RU2103298C1 |
POLYESTER ENAMEL | 2005 |
|
RU2287547C1 |
ENAMEL FOR WEATHER RESISTANT RADIATION-RESISTANT DECONTAMINATED ANTIFOULING MUSHROOM-RESISTANT COATING | 2018 |
|
RU2703636C1 |
Authors
Dates
2013-09-20—Published
2012-08-20—Filed