FIELD: metallurgy.
SUBSTANCE: water-diluting polymer composition for coatings includes epoxyamine resin, polyurethane hardener, modifying additive and deionised water; at that, as polyurethane hardener, there used is polyurethane containing 1.3-14.9 % of carbamide groups, 15.0-30.7 % of urethane groups, 0.33-1.80 % of biuretic groups, and as modifying additive there used is 2-mercaptobenzothiazole or 2-phenyl-4-chromenone, or 2,3-benzopyridine, or hexamethylenetetramine at the following component ratio, wt %: epoxyamine resin 5.8-8.8; polyurethane hardener 5.2-7.8; modifying additive 1.0-3.0; deionised water is the rest.
EFFECT: obtaining coatings with low moisture absorption, adhesion that is stable in water, stable physic and mechanical properties at thermal ageing, which are capable of being hardened at high speeds.
4 tbl, 1 ex
| Title | Year | Author | Number |
|---|---|---|---|
| POLYMERIC COMPOSITION FOR COVERS | 2005 |
|
RU2298573C2 |
| POWDER COMPOSITE FOR COVER | 2001 |
|
RU2194065C2 |
| POLYMERIC COMPOSITION FOR COATINGS | 2000 |
|
RU2179991C2 |
| POLYMERIC COMPOSITION FOR COATINGS | 2000 |
|
RU2179990C2 |
| COMPOSITION FOR COVER | 2003 |
|
RU2255100C1 |
| REINFORCED POLYURETHANE PULTRUDATES AND PRODUCTION THEREOF | 2012 |
|
RU2598070C2 |
| POLYURETHANE COMPOSITION FOR PRODUCING ANTI-NOISE COATINGS THROUGH MOULDING | 2009 |
|
RU2423403C2 |
| METHOD TO PRODUCE HIGH-POROSITY POLYMER MATERIAL | 2008 |
|
RU2377335C1 |
| METHOD FOR PRODUCING METHYLENED DIPHENYLDIAMINE USING A HETEROGENEOUS CATALYST | 2020 |
|
RU2743925C1 |
| POLYURETHANE COMPOSITION | 2003 |
|
RU2237069C1 |
Authors
Dates
2013-10-10—Published
2012-05-30—Filed