FIELD: metallurgy.
SUBSTANCE: method involves preliminary machining of initial raw material and further treatment of activated material with Na2CO3 soda solution. With that, preliminary machining is performed till the amount of energy adopted in the form of surface of coherent dissipation areas is achieved, which is equal to 25-27 kJ/mol of scheelite, and the amount of energy adopted in the form of microdeformations, which is equal to at least 2.3 kJ/mol of scheelite. Treatment with Na2CO3 soda solution is performed at the temperature of 99°C.
EFFECT: simplifying the development method owing to performing a leaching process at atmospheric pressure and reduced temperature.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ALKALINE DEVELOPMENT OF SCHEELITE CONCENTRATES | 2015 |
|
RU2610187C1 |
METHOD FOR OPENING TUNGSTENITE CONCENTRATES | 2012 |
|
RU2506330C1 |
METHOD FOR OPENING LOPARITE CONCENTRATES | 2012 |
|
RU2506333C1 |
METHOD OF OPENING PEROVSKITE CONCENTRATES | 2013 |
|
RU2525025C1 |
PROCESSING METHOD OF ARIZONITE AND ILMENITE CONCENTRATES | 2012 |
|
RU2490346C1 |
EUDIALYTE CONCENTRATE OPENING METHOD | 2018 |
|
RU2677571C1 |
METHOD OF EXTRACTING RARE-EARTH METALS AND PRODUCING GYPSUM PLASTER FROM ANHYDRITE | 2015 |
|
RU2607862C1 |
METHOD OF PRODUCING HIGH-STRENGTH GYPSUM | 2015 |
|
RU2613388C2 |
METHOD FOR PROCESSING TUNGSTEN CONCENTRATES | 2022 |
|
RU2785560C1 |
METHOD FOR RECOVERY OF TUNGSTEN FROM MANGANESE-TUNGSTATE CONCENTRATE | 1990 |
|
RU2024638C1 |
Authors
Dates
2013-10-27—Published
2012-10-10—Filed