FIELD: chemistry.
SUBSTANCE: binder contains in wt %: deeply oxidised tar - 30-40; high pressure polyethylene - 1.5-3.5; elementary sulphur - 0.15-0.45; straight run tar - to 100. Obtained binder possesses both high strength properties and sufficient elasticity. Expensive plasticisers are not used, cheaper and more available components are applied.
EFFECT: extension of assortment of binding materials for road construction works, corresponding to the level of main standard requirements to polymer-bitumen binders.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
BINDER (POLYETHYLENE-TAR BINDER WITH RUBBER CRUMB - PERB-R) FOR ROAD COVERING | 2012 |
|
RU2519214C1 |
RUBBER-BITUMEN ROAD BINDER FOR ASPHALT-CONCRETE MIXTURE | 2018 |
|
RU2707770C1 |
ROAD SURFACE BINDER (POLYMER-TAR BINDER) | 2009 |
|
RU2397187C1 |
BINDER (POLYMER-TAR-ASPHALTITE BINDER) FOR ROAD SURFACES | 2009 |
|
RU2394859C1 |
POLYMER-BITUMEN BINDER FOR ROAD SURFACE | 2021 |
|
RU2763726C1 |
RUBBER-POLYMER-BITUMEN BINDER AND METHOD FOR PRODUCTION THEREOF | 2020 |
|
RU2752619C1 |
POLYMER-BITUMEN BINDER FOR ROAD SURFACE AND METHOD FOR PRODUCTION THEREOF | 2016 |
|
RU2639902C1 |
POLYMER-BITUMEN BINDER AND METHOD FOR PRODUCTION THEREOF | 2012 |
|
RU2496812C1 |
POLYMER-BITUMEN BINDER AND METHOD FOR ITS PREPARATION | 2020 |
|
RU2754709C2 |
POLYMER-ASPHALT BINDER FOR ROAD SURFACE AND METHOD FOR PRODUCTION THEREOF | 2011 |
|
RU2477736C2 |
Authors
Dates
2014-06-10—Published
2012-12-26—Filed