FIELD: chemistry.
SUBSTANCE: method for the production of a polymer-bitumen binder is to be introduced into the bitumen at a temperature of 140-150°C a mixture of tar with a conventional viscosity at 80°C 60-300 s and the distillate fraction 540-610°C at a ratio of 3:1, in an amount of 30-60 wt % of the composition, and then a block copolymer of alkadiene and styrene in an amount of 3.0-3.5 wt %, until complete dissolution.
EFFECT: method increases the degree of homogenisation of bitumen compositions, thus widening the operating range thereof, which is characterised by softening temperature and brittleness temperature, reduces specific energy consumption when producing polymer-bitumen binder, as well as a cost thereof.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMER-ASPHALT BINDER FOR ROAD SURFACE AND METHOD FOR PRODUCTION THEREOF | 2011 |
|
RU2477736C2 |
POLYMER-BITUMEN BINDER WITH INCREASED RESISTANCE TO SHEAR DEFORMATIONS AND METHOD FOR PRODUCTION THEREOF | 2020 |
|
RU2765646C1 |
BINDER (POLYMER-TAR-ASPHALTITE BINDER) FOR ROAD SURFACES | 2009 |
|
RU2394859C1 |
BINDER (POLYETHYLENE-TAR BINDER WITH RUBBER CRUMB - PERB-R) FOR ROAD COVERING | 2012 |
|
RU2519214C1 |
ROAD SURFACE BINDER (POLYMER-TAR BINDER) | 2009 |
|
RU2397187C1 |
BINDER (POLYETHYLENE-TAR BINDER PETB) FOR ROAD COVERING | 2012 |
|
RU2519207C1 |
POLYMER-BITUMEN BINDER AND METHOD FOR PRODUCTION THEREOF | 2012 |
|
RU2496812C1 |
COMPOSITION AND METHOD FOR OBTAINING MODIFIED BITUMEN FOR ROAD CONSTRUCTION | 2022 |
|
RU2798340C1 |
POLYMER-BITUMEN BINDER AND METHOD FOR ITS PREPARATION | 2020 |
|
RU2754709C2 |
METHOD OF OBTAINING A POLYMER-BITUMEN ASTRINGENT FOR ROAD CONSTRUCTION | 2015 |
|
RU2618854C1 |
Authors
Dates
2017-12-25—Published
2016-09-02—Filed