FIELD: process engineering.
SUBSTANCE: invention relates to metal forming and may be used for complex-shape articles. Initial billet is formed in two steps. At first step, billet heated to deformation temperature is extruded. Note here that semi-finished product with surface with machining allowance. At second step, semi-finished product is deformed in cold state by reducing the surface with allowances and/or at extruding the cavities therein. Softening heat treatment is made between said steps.
EFFECT: products made from high-strength structural materials to high precision and low roughness.
4 dwg, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING A QUALITY FORGING OF A SWIVEL PIN OF A LORRY | 2016 |
|
RU2649627C2 |
METHOD OF MANUFACTURING THIN-WALLED AXISYMMETRIC SHELLS | 2016 |
|
RU2649477C1 |
METHOD FOR PRODUCTION OF HOLLOW PRODUCTS | 2007 |
|
RU2352430C2 |
METHOD OF PRODUCING THIN-WALL SHELLS | 2009 |
|
RU2419504C1 |
METHOD OF THIN-WALLED SHELLS WITH BOTTOM MAKING | 2015 |
|
RU2601364C1 |
METHOD OF PRODUCING THIN-WALL SHELLS | 2014 |
|
RU2556846C1 |
METHOD OF PRODUCING THIN-WALL SHELLS | 2009 |
|
RU2417854C1 |
METHOD FOR MANUFACTURING OF HOLLOW CYLINDER-CONE ITEMS WITH SOCKET AT ONE END | 2008 |
|
RU2391175C1 |
METHOD FOR PRODUCTION OF MOVABLE ABSORBER PIPE | 1992 |
|
RU2021074C1 |
METHOD OF MANUFACTURE OF HOLLOW ARTICLES | 2006 |
|
RU2312930C1 |
Authors
Dates
2014-08-10—Published
2012-12-07—Filed