FIELD: chemistry.
SUBSTANCE: ions of carbon with opposite charges interact with each other for 20-30 hours at a temperature of 850-950 °C in a high frequency electro-field in the range of frequencies of 40-80 kHz in the presence of iron as a catalyst. The process is carried out in a melt of salts, containing, wt %: SiC - 7.5-11.0; Na2CO3 or K2CO3 - 89.0-92.5. Applied is granulated iron, which has a size of granules 1-3 mm, in a quantity of 5-10% from the melt weight.
EFFECT: invention makes it possible to simplify the process of the diamond synthesis and its instrumentation, eliminate harmful and dangerous conditions.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
DIAMOND SYNTHESIS METHOD | 2011 |
|
RU2482060C1 |
METHOD OF PRODUCING SYNTHETIC DIAMONDS AND APPARATUS FOR REALISING SAID METHOD | 2011 |
|
RU2484016C1 |
METHOD OF OBTAINING DRY ZINC WHITE AND INSTALLATION FOR METHOD REALISATION | 2013 |
|
RU2542245C2 |
CLEANING METHOD OF ALUMINIUM REJECTS FROM IMPURITIES, AND FURNACE FOR METHOD'S IMPLEMENTATION | 2010 |
|
RU2440431C1 |
METHOD OF REMOVING IMPURITIES FROM ALUMINIUM AND FURNACE TO THIS END | 2011 |
|
RU2483128C2 |
METHOD OF PRODUCING ZINC POWDER AND PLANT TO THIS END | 2011 |
|
RU2457072C1 |
METHOD OF PRODUCING MAGNESIA CEMENT AND APPARATUS FOR REALISING SAID METHOD | 2011 |
|
RU2469004C1 |
METHOD TO PRODUCE ELECTRIC INSULATION COATING OF TRANSFORMER STEEL | 2011 |
|
RU2463384C1 |
PROCEDURE FOR REFINING WASTES OF ZINC FROM IMPURITIES AND FURNACE FOR IMPLEMENTATION OF THIS PROCEDURE | 2010 |
|
RU2436854C1 |
METHOD OF DIAMOND SYNTHESIS | 1999 |
|
RU2181795C2 |
Authors
Dates
2014-10-20—Published
2013-03-22—Filed