FIELD: chemistry.
SUBSTANCE: method of obtaining lead stearate includes the interaction of stearic acid with a water suspension of lead oxide with heating and intensive mixing with further filtration, drying, pre-packing and packing. Water, acetic acid as a catalyst and lead oxide are loaded with obtaining the water suspension of lead oxide. After that, it is heated to a temperature of 75-80°C and stearic acid is added, circulation is performed for 60-90 min at a temperature of thermal processing to 75-80°C. After that, the suspension of lead stearate is transferred into a condition of a stable emulsion, exposed at the said temperature for 100-120 min to pH of the solution being 4.0-6.0, acidic number to 0.5 mg and the content of the main substance 26-28%, with the following addition of water, mixing and filtration. The product drying is performed by hot air at a temperature of 60-80°C.
EFFECT: simplification of the technological process and an increase of the final product quality.
2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING ZINC STEARATE | 2012 |
|
RU2516663C1 |
METHOD OF OBTAINING DIBASIC LEAD STEARATE, POLYVINYL CHLORIDE STABILISER | 2012 |
|
RU2506253C1 |
METHOD FOR PRODUCTION OF CALCIUM-ZINC STABILIZER | 2017 |
|
RU2672262C1 |
METHOD OF PRODUCING METAL-CONTAINING LUBRICANTS FOR PVC COMPOSITION | 2017 |
|
RU2642075C1 |
METHOD OF PRODUCING METAL-CONTAINING LUBRICANT FOR PVC COMPOSITION | 2017 |
|
RU2644898C1 |
METHOD FOR PRODUCING CARBOXYLATES OF METALS OF VARIABLE VALENCE | 2016 |
|
RU2618858C1 |
METHOD OF OBTAINING THE LEAD STEARATE DIBASIC - POLYVINYLCHLORIDE STABILIZER | 2016 |
|
RU2656477C1 |
METHOD FOR OBTAINING PLASTICISER FOR POLYVINYL CHLORIDE COMPOSITION | 2017 |
|
RU2643996C1 |
METHOD FOR PRODUCTION OF COMPOSITION FOR OIL-BENZINE-RESISTANT PLASTICATE | 2016 |
|
RU2631880C1 |
METHOD OF PRODUCING CALCIUM-ZINC STEARATE | 2019 |
|
RU2705719C1 |
Authors
Dates
2014-11-20—Published
2013-03-04—Filed