FIELD: metallurgy.
SUBSTANCE: powder composition from graphite, resin and additives is crushed and mixed at temperature of 25÷35°C below temperature of resin melting during 20÷30 minutes, then it is pressed.
EFFECT: improving strength and conductivity.
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION METHOD OF SLIDING CONTACTS | 2013 |
|
RU2529605C1 |
METHOD FOR OBTAINING OF ELECTROTECHNICAL ARTICLES FROM THE POWDER COMPOSITIONS BASED ON CARBON | 2017 |
|
RU2652302C1 |
METHOD OF PRODUCING GRAPHITE FIBER ARTICLES | 2015 |
|
RU2613245C1 |
METHOD OF PRODUCING ELECTROTECHNICAL ARTICLES FROM POWDER COMPOSITIONS BASED ON CARBON | 2019 |
|
RU2707001C1 |
METHOD OF MANUFACTURE OF CONTACT SLIPPERS | 2004 |
|
RU2267411C1 |
PRODUCTION OF ELECTRICAL CARBON ARTICLES | 2013 |
|
RU2560619C2 |
METHOD OF PRODUCING ELECTRIC CARBON ARTICLES | 2015 |
|
RU2602569C1 |
PRESSING METHOD OF ELECTROTECHNICAL ITEMS FROM POWDER COMPOSITIONS BASED ON CARBON | 2014 |
|
RU2567083C1 |
PRODUCTION OF ELECTRICAL CARBON ARTICLES | 2013 |
|
RU2560490C2 |
METHOD OF MANUFACTURE OF ELECTRIC VEHICLE CURRENT COLLECTOR CONTACT SLIPPER | 2001 |
|
RU2207962C1 |
Authors
Dates
2014-11-27—Published
2013-07-31—Filed