FIELD: chemistry.
SUBSTANCE: method includes polishing component of copper-containing alloy in electrolyte, used as anode, and synchronous application of copper coating on steel component, used as cathode. Voltage 250-340 V is supplied to cathode and anode with electrolyte temperature 60-90°C. Electrolyte is used in form of water solution, which contains ammonium chloride, ammonium fluoride and mono-, di-, tri-substituted ammonium citrate or their mixture.
EFFECT: polishing of active anode to mirror lustre with synchronous covering of steel cathode surface with copper.
1 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR ELECTROLYTE-PLASMA TREATMENT OF METAL SURFACE | 2014 | 
 | RU2550393C1 | 
| METHOD OF TREATING METAL SURFACE | 2014 | 
 | RU2550436C1 | 
| COPPER-PLATING ELECTROLYTE | 0 | 
 | SU953012A1 | 
| PROCESS OF ELECTROCHEMICAL MACHINING OF SURFACES OF METAL ARTICLES | 1998 | 
 | RU2155828C2 | 
| METHOD OF BIMETAL WIRE PRODUCING | 2015 | 
 | RU2605736C2 | 
| METHOD FOR ELECTROLYTIC-PLASMA POLISHING OF PART IN ALTERNATING MAGNETIC FIELD | 2023 | 
 | RU2821036C1 | 
| METHOD FOR ELECTROLYTIC-PLASMA POLISHING OF PART IN ALTERNATING MAGNETIC FIELD AT LOW PRESSURE | 2023 | 
 | RU2820693C1 | 
| BRIGHT COPPER PLATING ELECTROLYTE | 2002 | 
 | RU2215829C1 | 
| ELECTROLYTE FOR DEPOSITING TIN-BISMUTH ALLOY | 0 | 
 | SU1712469A1 | 
| ELECTROLYTE FOR BRIGHT COPPER PLATING | 2002 | 
 | RU2237754C2 | 
Authors
Dates
2015-01-10—Published
2013-06-28—Filed