FIELD: construction.
SUBSTANCE: nanostructured wood-mineral composite material, including a wood filler, a binder and water, additionally contains a reinforcing filler from basalt with average particle size of 50-100 nm, and wood filler is wood of coniferous species in the form of microdispersed particles of wood with average particle size of 1-2 mcm at the following ratio of components, wt %: wood 40-55, basalt 30-40, slaked lime 10-15, water - balance.
EFFECT: increased strength, water resistance.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
WOOD BARK-BASED NANOCOMPOSITE STRUCTURAL MATERIAL | 2015 |
|
RU2591063C1 |
RAW MIXTURE FOR WOOD-MINERAL ARTICLES MANUFACTURE | 0 |
|
SU1726433A1 |
SAWDUST CHIPBOARD | 2015 |
|
RU2608531C2 |
RAW MATERIAL MIXTURE FOR PRODUCTION OF HEAT INSULATING LIGHT CONCRETE | 2008 |
|
RU2377210C2 |
METHOD OF PRODUCING CEMENT-CHIP BLOCKS | 2014 |
|
RU2578077C1 |
METHOD FOR OBTAINING AN ADDITIVE FOR MODIFYING OIL BITUMENS | 2021 |
|
RU2756811C1 |
RAW MATERIALS MIXTURE FOR MANUFACTURE OF WOOD-MINERAL BUILDING MATERIALS | 2000 |
|
RU2191756C2 |
METHOD OF OBTAINING AND COMPOSITION OF ACTIVATED REINFORCED MINERAL POWDER | 2014 |
|
RU2568620C1 |
METHOD OF MAKING BEARING WALLS | 2023 |
|
RU2816138C1 |
WOOD-POLYMERIC COMPOSITION | 1992 |
|
RU2049662C1 |
Authors
Dates
2015-02-20—Published
2013-11-27—Filed