FIELD: construction.
SUBSTANCE: method for producing the concrete aggregate includes preparation of mass based on low-melting clays, capable to swell under conditions of heat treatment, its hydration up to 17-23%, formation of granules, melting into the surface of moulded granules of the crushed cement clinker sieved through mesh No. 5, drying, calcining at a temperature of 1100°C, cooling.
EFFECT: increase of the bond strength of aggregate with cement stone.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF FILLER FOR CONCRETE | 2015 |
|
RU2572858C1 |
METHOD OF PRODUCING AGGREGATE FOR CONCRETE | 2016 |
|
RU2634930C1 |
METHOD OF DECORATIVE FILLER MANUFACTURING | 2007 |
|
RU2345054C1 |
METHOD FOR PRODUCING AGGREGATE FOR CONCRETE | 2016 |
|
RU2616012C1 |
METHOD OF MANUFACTURING OF DECORATIVE FILLING MATERIAL | 2007 |
|
RU2343127C1 |
METHOD OF MAKING CLAYDITE GRAVEL | 2011 |
|
RU2459774C1 |
METHOD OF MAKING CLAYDITE GRAVEL | 2012 |
|
RU2491242C1 |
METHOD OF MAKING CLAYDITE GRAVEL (VERSIONS) | 2012 |
|
RU2486149C1 |
METHOD TO MANUFACTURE HAYDITE GRAVEL | 2013 |
|
RU2514031C1 |
METHOD OF PRODUCING POROUS AGGREGATE (VERSIONS) | 2011 |
|
RU2439013C1 |
Authors
Dates
2015-03-10—Published
2014-02-25—Filed