FIELD: construction.
SUBSTANCE: clay mixture is prepared, wetted, granules are formed, dried, burned and cooled. Prepared on the bases of low - melting clays mass is damped up to 17-23%, formed grains are dried reaching humidity of 1-6%, burned at 1100°C within 10-20 minutes, cooled down to 20-50°C, damped by immersion into the vessel with water solution of sodium chloride and exposed for 24 hours. Been reached out from the capacity, grains are dried reaching humidity rate of 5-8%, burned at 1100°C within 10-20 minutes and cooled.
EFFECT: enhanced cold resistance property of keramzite gravel and its improved ornamentality.
2 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DECORATIVE FILLER MANUFACTURING | 2007 |
|
RU2345054C1 |
METHOD OF MAKING CLAYDITE GRAVEL (VERSIONS) | 2012 |
|
RU2486149C1 |
METHOD FOR PRODUCING CONCRETE AGGREGATE | 2014 |
|
RU2543774C1 |
METHOD OF MAKING CLAYDITE GRAVEL | 2011 |
|
RU2459774C1 |
METHOD FOR PRODUCTION OF HAYDITE GRAVEL | 2008 |
|
RU2366629C1 |
METHOD OF MAKING CLAYDITE GRAVEL | 2012 |
|
RU2491242C1 |
METHOD OF PRODUCTION OF HAYDITE GRAVEL | 2008 |
|
RU2366630C1 |
METHOD OF PRODUCTION OF KERAMZITE GRAVEL | 2008 |
|
RU2359932C1 |
METHOD OF PRODUCING POROUS AGGREGATE | 2010 |
|
RU2449961C1 |
METHOD TO MANUFACTURE HAYDITE GRAVEL | 2013 |
|
RU2514031C1 |
Authors
Dates
2009-01-10—Published
2007-06-18—Filed