FIELD: woodworking industry.
SUBSTANCE: test sample is preliminary weighed, placed on the distilled water meniscus formed in the vessel. Then the sample is kept for at least 24 hours and removed from the vessel. Then the repeated weighting of the sample is carried out.
EFFECT: providing the possibility to assess the quality of protective and decorative coating on water resistance with minimal costs and obtaining the results in a simpler way.
2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DETERMINING WATER RESISTANCE OF TEXTILE PRODUCTS, LEATHER AND COATINGS | 2015 |
|
RU2592628C1 |
ATMOSPHERE RESISTANT AQUEOUS DISPERSIVE COMPOSITION | 1999 |
|
RU2162477C1 |
MAGNETIC MATERIAL CORROSION RATE DETERMINATION METHOD | 0 |
|
SU991266A1 |
WASHING COMPOSITION FOR PURIFICATION OF SOLID SURFACE | 0 |
|
SU1625894A1 |
MEANS AND METHOD FOR PROTECTION OF NON-METALLIC MATERIALS AGAINST BIOFAILURES | 2002 |
|
RU2211759C1 |
EVALUATION METHOD OF EFFECTIVENESS OF SOLVENTS OF ORGANIC DEPOSITS | 2010 |
|
RU2429344C1 |
AGENT FOR PROTECTION OF WOOD AND PAINTWORK MATERIALS FROM BIODEGRADATION, METHOD OF PREPARATION THEREOF AND BIODEGRADATION PROTECTION METHOD | 1999 |
|
RU2158677C1 |
MATERIAL DENSITY CHECKING METHOD | 2002 |
|
RU2233447C1 |
EPOXIDE COMPOSITION FOR BIOCIDAL COVERING | 2001 |
|
RU2190648C1 |
METHOD FOR ASSESSING THE QUALITY OF PAINT COATINGS APPLIED ON THE SURFACE OF PRODUCTS | 2022 |
|
RU2795376C1 |
Authors
Dates
2015-07-20—Published
2014-03-03—Filed