FIELD: chemistry.
SUBSTANCE: method includes first wet grinding glass ceramic to obtain a highly concentrated slurry with density of 2.10-2.13 g/cm3, fineness (residue on a 0.063 mm sieve) of 5.0-7.5% and content of particles with a size smaller than 5 mcm of 30-35%. Workpieces with an arbitrary shape are moulded and subjected to re-treatment in a slurry with density of 2.10-2.14 g/cm3, fineness of 5.5-6.9% and content of particles with a size smaller than 5 mcm of 30-39%. Articles are then moulded and heat treated.
EFFECT: shorter duration of moulding, low water absorption and high strength of the glass ceramic material of cowlings.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING ARTICLES FROM GLASS-CERAMIC MATERIAL OF LITHIUM ALUMINOSILICATE COMPOSITION | 2021 |
|
RU2768554C1 |
METHOD OF MAKING ANTENNA CAP FROM GLASS-CERAMIC LITHIUM ALUMINOSILICATE MIXTURE | 2006 |
|
RU2326094C1 |
METHOD OF BEDDER-SUPPORTS MANUFACTURING FOR GLASS-CERAMIC PRODUCTS BAKEOUT | 2016 |
|
RU2634771C1 |
METHOD OF MAKING CERAMIC ARTICLES | 2018 |
|
RU2707618C1 |
METHOD OF PRODUCTION OF ARTICLES FROM SINTERED GLASS CRYSTALLINE MATERIAL OF LITHIUM-ALUMO- SILICATE COMPOSITION | 2002 |
|
RU2222505C1 |
METHOD FOR MANUFACTURING CONTAINERS FOR HEAT TREATMENT OF LOOSE MATERIALS | 2019 |
|
RU2715139C1 |
METHOD OF MAKING ANTENNA DOME FROM GLASS-CERAMIC OF LITHIUM-ALUMINOSILICATE COMPOSITION | 2013 |
|
RU2513389C1 |
PRODUCTION OF GLASS-CERAMIC MATERIAL OF CORDIERITE COMPOSITION | 2014 |
|
RU2566840C1 |
METHOD OF PREPARING PRODUCTS FROM SINTERED GLASS CRYSTALLINE LITHIUM ALUMOSILICATE MATERIAL | 1999 |
|
RU2170715C2 |
METHOD OF MAKING GLASS-CERAMIC ANTENNA CAP | 2009 |
|
RU2414438C1 |
Authors
Dates
2015-11-10—Published
2014-10-06—Filed