FIELD: metallurgy.
SUBSTANCE: method of production of surface-nanostructured metal includes metal restoration from initial metal containing solid material by treatment by vapours of silicone liquid for rendering water-repellent in form of low-molecular oligo organohydridesiloxanes with further annealing in dehydrated natural gas. Metal restoration is performed at temperature from 320 to 400°C using natural gas as gas carrying vapours of silicone liquid for rendering water-repellent, and annealing is performed at temperature from 500 to 695°C.
EFFECT: reduced method toxicity.
2 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
GEL-LIKE ORGANOSILICON COMPOSITION | 1997 |
|
RU2127746C1 |
METHOD FOR SHUTOFF OF INFLOW OF FORMATION WATER | 0 |
|
SU1803532A1 |
METHOD OF PRODUCING METALLIC MAGNETIC COATINGS | 2018 |
|
RU2710611C1 |
POROUS MAGNETIC SORBENT | 2002 |
|
RU2226126C1 |
METHOD FOR PRODUCTION OF COMPOSITE METAL-CERAMIC COATING AT VALVE METALS AND THEIR ALLOYS | 2013 |
|
RU2543659C1 |
METHOD OF PRODUCING HYDROPHOBIC ADSORBENT FOR CLEANING NATURAL WATERS AND SEWAGE FROM OIL PRODUCTS | 2011 |
|
RU2480277C1 |
METHOD FOR PRODUCING IRON POWDER | 2002 |
|
RU2231420C1 |
MONODISPERSE COLLOIDAL AQUEOUS SOLUTION OF SILVER IONS WITH ANTIMICROBIAL AND ANTITOXIC ACTION (VERSIONS) AND METHOD OF ITS PRODUCTION | 2015 |
|
RU2609176C2 |
METHOD FOR ANTICORROSION TREATMENT OF ALUMINIUM SURFACE | 2017 |
|
RU2693278C2 |
CAST IRON ALLOYING WITH VANADIUM | 2012 |
|
RU2520929C2 |
Authors
Dates
2015-12-10—Published
2014-07-01—Filed