FIELD: chemistry.
SUBSTANCE: method for preparation of glass fusion charge includes mixing of raw material components, introduction of binding agent - 40% of liquid glass solution in quantity 5.0 wt % with addition of superplasticiser MB-1 in quantity 0.5 wt %. Briquetting is realised under pressing pressure 5.0 MPa.
EFFECT: increase of solution wetting ability and increased rate of solid phase reactions of fusion charge components, reduction of briquetting pressure.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING GLASS BATCH | 2011 |
|
RU2464240C1 |
METHOD FOR BRIQUETTING IRON-CONTAINING WASTES IN FORM OF SCALE | 2019 |
|
RU2705483C1 |
METHOD OF MAKING GLASS BATCH | 2011 |
|
RU2472720C2 |
IRON-CONTAINING MATERIAL PROCESSING METHOD | 2011 |
|
RU2466196C1 |
BRIQUETTE FOR METALLURGICAL PRODUCTION, BRIQUETTE FOR WASHING OUT HEARTH OF BLAST FURNACE AND METHOD FOR MAKING SUCH BRIQUETTES | 2001 |
|
RU2183679C1 |
METHOD OF PREPARING MIXTURE FOR SYNTHESIS OF WOLLASTONITE AND COMPOSITION THEREOF | 2008 |
|
RU2380340C1 |
METHOD TO PREPARE IRON ORE FOR METALLURGICAL PROCESSING | 2010 |
|
RU2463362C2 |
METHOD OF MAKING PELLETS FROM ORES AND CONCENTRATES OF FERROUS METALS | 2011 |
|
RU2484151C1 |
METHOD OF BRIQUETTING CARBON REDUCING AGENTS | 2017 |
|
RU2669940C1 |
METHOD OF PREPARING BURDEN FOR MELTING FLUORIDE-OXIDE FLUXES | 0 |
|
SU1786105A1 |
Authors
Dates
2015-12-20—Published
2014-11-19—Filed