FIELD: metallurgy.
SUBSTANCE: proposed mix contains the following components, in wt %: marble - 19.0-21.0, ilmenite - 19.0-21.0, ferromanganese - 13.0-15.0, rutile - 28.5-29.5, kaolin - 4.0-6.0, talc - 9.0-11.0, cellulose - 1.0-2.0, potash - 0.5-1.5 and mechanically activated powder of the electrode mix MP3 - 0.25-0.45 with particle size of up to 20 mcm.
EFFECT: higher welding properties and the joint built-up metal.
4 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION OF CHARGE FOR COATING ELECTRODES DESIGNED FOR WELDING LOW CARBON STEEL | 2008 |
|
RU2383418C1 |
COMPOSITION OF ELECTRODE COATING | 1994 |
|
RU2033912C1 |
ELECTRODE COATING COMPOSITION | 2002 |
|
RU2217286C1 |
ELECTRODE COATING COMPOSITION | 2002 |
|
RU2217287C1 |
ELECTRODE COATING COMPOSITION | 2012 |
|
RU2510317C1 |
COMPOSITION OF ELECTRODE COATING | 1999 |
|
RU2155657C1 |
ELECTRODE COATING COMPOSITION | 2001 |
|
RU2217285C2 |
ELECTRODE COATING COMPOSITION | 0 |
|
SU963771A1 |
COMPOUND OF ELECTRODE COATING | 1992 |
|
RU2056991C1 |
ELECTRODE COATING COMPOSITION | 2007 |
|
RU2353493C2 |
Authors
Dates
2016-03-27—Published
2014-07-02—Filed