FIELD: machine building.
SUBSTANCE: invention relates to mandrel, used in piercing mill, piercing and rolling workpiece. Piercing mandrel consists of housing and coating based on iron and iron oxide sprayed on housing surface, wherein sprayed coating contains the following, wt%: C 0.015-0.6, Si 0.05-0.5, Mn 0.1-1.0, Cu 0-0.3, iron, iron oxide and impurities - the rest, wherein iron oxide content in coating ranges from 55-80 vol%.
EFFECT: higher efficiency of hollow tubular billets production by obtaining mandrels with high-quality coating.
6 cl, 2 tbl, 3 dwg, 1 ex
Title | Year | Author | Number |
---|---|---|---|
DISK MILL MANDREL | 2013 |
|
RU2584620C1 |
PIERCING AND ROLLING MANDREL, METHOD OF ITS RECONDITIONING AND PROCESS LINE TO THIS END | 2008 |
|
RU2446024C2 |
STEEL PIPE FOR HIGH-PRESSURE FUEL PIPE AND HIGH-PRESSURE FUEL PIPE COMPRISING IT | 2015 |
|
RU2650466C2 |
METHOD OF MAKING MANDREL FOR ROLLING WITH PIERCING | 2013 |
|
RU2588937C2 |
SYSTEM OF EQUIPMENT FOR PIERCING AND ROLLING MANDREL PRODUCTION | 2013 |
|
RU2600771C2 |
THICK-WALLED STEEL ARTICLE MANUFACTURING PROCESS LINE AND THE THICK-WALLED STEEL ARTICLE MANUFACTURING METHOD FROM THE HIGH-STRENGTH STAINLESS STEEL IN THE PROCESS LINE | 2014 |
|
RU2660474C2 |
CU-CONTAINING NON-TEXTURED ELECTRICAL STEEL SHEET AND THE SHEET PRODUCTION METHOD | 2020 |
|
RU2790231C1 |
SEAMLESS STEEL PIPE AND METHOD OF ITS PRODUCTION | 2016 |
|
RU2706257C1 |
METHOD OF MAKING MANDREL FOR PIERCING ROLLING | 2013 |
|
RU2598414C2 |
TWO-PHASE STAINLESS STEEL AND ITS MANUFACTURING METHOD | 2017 |
|
RU2698235C1 |
Authors
Dates
2016-12-20—Published
2013-08-01—Filed