FIELD: chemistry.
SUBSTANCE: as initial component, Aerosil (SiO2) nanoscale powder with a surface area of 350-380 m2/g is selected and dried in vacuo for 1-3 hours. Iron oxide and lithium oxide films with a thickness of 1-3 nm are coated on aerosil powder by means of the MLT method to achieve the stoichiometric composition Li2FeSiO4 and the diffusion mixing of the resulting composition Li2FeSiO4 is carried out at 300°C to 500°C for 8-15 hours.
EFFECT: invention allows to obtain a cathode material having a high specific surface area and high specific capacity, with the uniform distribution of the chemical composition in the total powder volume and the defect-free crystal structure.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING A THIN FILM CATHODE | 2016 |
|
RU2623104C1 |
METHOD FOR PRODUCING NANOCOMPOSITION POWDER ANODE MATERIALS FOR LITHIUM-ION ACCUMULATORS | 2016 |
|
RU2634561C1 |
METHOD OF NANOCRYSTALLINE COMPOSITE CATHODE MATERIALS LiFeMSiO/C | 2012 |
|
RU2522918C2 |
METHOD OF OBTAINING NANOCRYSTALLINE COMPOSITE CATHODE MATERIALS LiFeMSiO/C | 2013 |
|
RU2522939C1 |
METHOD OF PRODUCING COMPOSITE OXIDE OF LITHIUM AND COBALT | 2016 |
|
RU2637222C2 |
METHOD OF PRODUCING CATHODE MATERIAL FOR LITHIUM-ION BATTERIES | 2016 |
|
RU2638316C1 |
METHOD FOR OBTAINING LITHIUM-IRON-PHOSPHATE | 2013 |
|
RU2585646C2 |
METHOD OF PRODUCING CATHODE MATERIAL FOR LITHIUM-ION BATTERIES | 2017 |
|
RU2643164C1 |
PRODUCTION OF SUPERDISPERSED POWDERS OF VARIOUS OXIDES WITH NARROW SEPARATION OF PARTICLES BY SIZES | 2014 |
|
RU2569535C1 |
METHOD FOR LIQUID-PHASE SYNTHESIS OF NANOCERAMIC MATERIALS IN THE LaO-SrO-Ni(Co,Fe)O SYSTEM FOR CREATING CATHODE ELECTRODES OF A SOLID OXIDE FUEL CELL | 2022 |
|
RU2784880C1 |
Authors
Dates
2017-04-06—Published
2015-12-22—Filed