FIELD: metallurgy.
SUBSTANCE: for carrying out the leaching process of pentlandite-pyrrhotite concentrate at a temperature of 90-105°C with the feeding of sulfuric acid and sodium sulfate into the autoclave, the oxygen partial pressure is increased from more than 0.5 to 1.5 MPa. The oxidated pulp is delivered for separation to solid and liquid phases. The metal containing solution is sent for processing, and solid phase - for floatation, during it sulfur sulphide concentrate and tails of dump quality are produced, to them maximum 5% of non-ferrous and maximum 5-15% of precious metal are transferred. The method is applicable for the leaching of pyrrhotite-pentlandite concentrates at any nickel content in the range of 0.5-20%.
EFFECT: intensification of the leaching process.
2 cl, 3 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
PROCESSING METHOD OF SULPHIDE PYRRHOTINE-PENTLANDITE CONCENTRATES CONTAINING PRECIOUS METALS | 2014 |
|
RU2573306C1 |
METHOD OF PROCESSING SULPHIDE CONCENTRATES CONTAINING PYRRHOTINE, PYRITE, CHALCOPYRITE, PENTLANDITE AND PRECIOUS METALS | 2019 |
|
RU2712160C1 |
METHOD OF OXIDIZING PRESSURE LEACHING OF POLYMETALLIC FERROSULFIDE MATERIALS CONTAINING PRECIOUS METALS | 1997 |
|
RU2117709C1 |
METHOD OF PROCESSING SULFIDE POLYMETALLIC PIRRHOTINE CONTAINING MATERIALS | 1992 |
|
RU2016102C1 |
METHOD FOR PROCESSING OF DIFFICULT-TO-OPEN SULFIDE PYRRHOTITE- CONTAINING MATERIALS PASSIVATED BY SULFIDE OXYGEN CORROSION PRODUCTS | 2002 |
|
RU2235139C1 |
METHOD FOR REPROCESSING OF SULFIDE CONCENTRATE WITH HIGH CONTENT OF PYRROTINE | 2002 |
|
RU2245377C2 |
METHOD FOR PROCESSING NICKEL-BEARING PYRRHOTINE CONCENTRATES | 0 |
|
SU1126620A1 |
METHOD FOR PROCESSING SULPHIDE POLYMETALLIC MATERIALS CONTAINING PLATINUM METALS (VARIANTS) | 2017 |
|
RU2667192C1 |
METHOD FOR FLOTATION OF PENTLANDITE FROM POLYMETALLIC PYRRHOTINE-CONTAINING MATERIALS | 1997 |
|
RU2108168C1 |
METHOD OF PROCESSING PYRRHOTITE CONTAINING MATERIALS | 0 |
|
SU1638188A1 |
Authors
Dates
2017-07-25—Published
2016-05-13—Filed