FIELD: metallurgy.
SUBSTANCE: method for production of titanium powder includes exposure of titanium wastes to distilled water at 250 Hz pulse repetition rate, 150 V electrodes voltage and capacitance of discharge capacitors at 65 mcF.
EFFECT: production of titanium powder with regular spherical shape particles with average size of 33,12 mcm and with low energy costs, enironmental cleanliness of the process and decrease of fire and explosion hazard.
6 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF W-Ni-Fe PSEUDO-ALLOY POWDER BY METHOD OF ELECTRIC EROSION DISPERSION IN DISTILLED WATER | 2017 |
|
RU2683162C2 |
METHOD OF PRODUCING SPHERICAL TITANIUM POWDERS FROM “OT4” ALLOY WASTES IN DISTILLED WATER | 2024 |
|
RU2824646C1 |
METHOD OF PRODUCING TITANIUM POWDERS OF SPHERICAL SHAPE FROM WASTES OF OT4 ALLOY IN PROPYL ALCOHOL | 2024 |
|
RU2824012C1 |
METHOD OF PRODUCING METALLIC NANOPOWDER FROM LEAD BRONZE WASTES IN DISTILLED WATER | 2018 |
|
RU2710707C1 |
METHOD FOR PRODUCING ALUMINIUM NANOPOWDERS | 2015 |
|
RU2612117C1 |
METHOD FOR PRODUCING FINE-GRAINED CORUNDUM | 2016 |
|
RU2664149C2 |
METHOD OF PRODUCING COPPER NANOPOWDER FROM WASTES | 2014 |
|
RU2597445C2 |
METHOD OF PRODUCING STEEL POWDERS ELECTROEROSION DISPERSION OF WASTES OF BALL BEARING STEEL IN WATER | 2015 |
|
RU2597443C1 |
METHOD OF PRODUCING COPPER POWDER FROM WASTES | 2014 |
|
RU2599476C2 |
METHOD FOR PRODUCING LEAD-ANTIMONY POWDER FROM “ССу3” ALLOY WASTE IN DISTILLED WATER | 2022 |
|
RU2782593C1 |
Authors
Dates
2017-09-25—Published
2016-11-11—Filed