FIELD: metallurgy.
SUBSTANCE: steel contains, wt %: carbon 0.10-0.20, silicon 0.02-0.40, manganese 0.02-0.6, chrome 2.0-2.5, nickel 1.25-2.0, molybdenum 0.35-0.7, vanadium 0.10-0.15, copper 0.005-0.03, cobalt 0.001-0.03, sulfur 0.0005-0.003; phosphorus 0.0005-0.004; arsenic 0.001-0.004; antimony 0.001-0.004; stannum 0.001-0.004; hydrogen 0.00001-0.00012, aluminium 0.015-0.035, nitrogen 0.0001-0.008, oxygen 0.0001-0.0030, bismuth 0.001-0.004, lead 0.001-0.004, iron-the rest.
EFFECT: improved service and technological properties of steel, yield point and strength limit, provision of guaranteed low values of critical brittleness temperature, increased resistance to embrittlement at thermal action and neutron irradiation.
4 cl
Title | Year | Author | Number |
---|---|---|---|
HEAT-RESISTANT AND RADIATION-RESISTANT STEEL | 2016 |
|
RU2633408C1 |
HEAT- AND RADIATION-RESISTANT STEEL | 2021 |
|
RU2773227C1 |
HIGHLY STRONG HEAT- AND RADIATION-RESISTANT STEEL | 2021 |
|
RU2777681C1 |
COLD-RESISTANT STEEL FOR SPENT NUCLEAR MATERIAL STORAGE DEVICES | 2022 |
|
RU2804233C1 |
WELDING WIRE FOR AUTOMATIC WELDING OF HEAT-RESISTANCE PEARLITIC STEELS | 2013 |
|
RU2530611C1 |
COLD-RESISTANT STEEL | 2017 |
|
RU2648426C1 |
STEEL | 2011 |
|
RU2477335C1 |
WELDING WIRE FOR AUTOMATIC WELDING OF HEAT-RESISTANCE PEARLITIC STEELS | 2010 |
|
RU2451588C2 |
LOW-ACTIVATED FIRE-RESISTANT RADIATION-RESISTANT STEEL | 2013 |
|
RU2515716C1 |
STEEL | 2010 |
|
RU2441940C1 |
Authors
Dates
2017-11-07—Published
2016-12-28—Filed