FIELD: metallurgy.
SUBSTANCE: passivation of aluminium nano-powder with air containing water vapours, then, the passivated aluminium nano-powder is heated to 300-400°C in air atmosphere at a heating rate of 10 to 30°C/min and kept at this temperature for 30 minutes.
EFFECT: increase of thermal oxidation effect.
3 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ACTIVATING ALUMINUM NANOPOWDER | 2018 |
|
RU2687121C1 |
METHOD FOR OBTAINING NANOPOWDERS OF METALS WITH INCREASED STORED ENERGY | 2013 |
|
RU2535109C2 |
METHOD FOR MODIFYING MICRO AND NANOPOWDERS OF ALUMINUM | 2017 |
|
RU2657677C1 |
METHOD OF PRODUCING GAS ABSORBER FROM TITANIUM POWDER | 2010 |
|
RU2424085C1 |
COPPER-CONTAINING TITANIUM ALLOY AND METHOD OF ITS PRODUCTION | 2023 |
|
RU2820186C1 |
METHOD FOR PRODUCTION OF COMPACT FINE-GRAINED CERAMIC USING ALUMINUM, CERIUM AND CIRCONIUM OXIDE BASED COMPOSITE NANO-POWDER SYNTHESIZED BY MODIFIED SOL GEL METHOD | 2015 |
|
RU2610483C1 |
CATALYST OF OIL FRACTIONS HYDROFINING AND METHOD OF ITS PRODUCTION | 2010 |
|
RU2445163C1 |
METHOD OF PRODUCING COPPER NANOPOWDER | 2015 |
|
RU2585582C1 |
METHOD OF PRODUCING NANOPOROUS MATERIAL FOR SENSITIVE ELEMENTS OF GAS SENSORS AND NANOPOROUS MATERIAL OBTAINED USING SAID METHOD | 2015 |
|
RU2614146C1 |
METHOD FOR PRODUCING LUMINESCENT NANOSCALE OPTICALLY TRANSPARENT MgALOCERAMICS | 2021 |
|
RU2775450C1 |
Authors
Dates
2017-12-06—Published
2016-10-31—Filed