FIELD: coal industry.
SUBSTANCE: invention relates to the field of coal enrichment, in particular to the production of high-quality coal coke and high-caloric heat-treated solid fuel for metallurgy, power industry and other industries. Prior to thermal treatment of coal, extreme cooling of coal is carried out to the temperature of -10 to -12 °C. Then, the coal is heated in the fluidized bed furnace in three stages. At the first stage, heating is carried out to the temperature from 120 up to 130 °C, in the second stage to the temperature from 280 up to 300 °C, in the third stage to the temperature from 500 up to 550°C.
EFFECT: technical result is to increase the yield of the coke residue at the decrease in its ash content.
1 cl, 1 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF COAL CONVERSION | 2009 |
|
RU2401295C1 |
METHOD OF THERMAL COAL ENRICHMENT | 2015 |
|
RU2637551C2 |
METHOD FOR PRODUCING CARBON SORBENT IN A FLUIDIZED BED | 2022 |
|
RU2777640C1 |
METHOD OF PREPARING SEMICOKE | 2000 |
|
RU2169166C1 |
COAL THERMAL BENEFICATION AND DEVICE TO THIS END | 2012 |
|
RU2518624C2 |
METALLURGICAL SEMICOKE MANUFACTURING PROCESS | 2004 |
|
RU2275407C1 |
METHOD OF PARTIALLY BRIQUETTED CHARGE PREPARATION FOR COKING | 2007 |
|
RU2348680C1 |
COAL PROCESSING METHOD | 2018 |
|
RU2722557C2 |
METALLURGICAL MEDIUM-TEMPERATURE COKE PRODUCTION PROCESS | 2005 |
|
RU2288937C1 |
METHOD FOR PRODUCING CARBON ADSORBENT | 1993 |
|
RU2014883C1 |
Authors
Dates
2018-05-07—Published
2017-07-18—Filed