FIELD: metal rolling.
SUBSTANCE: invention relates to the technology of thermo-friction cutting with a disk saw heated to temperature of 1150–1250 °C from pipe rolling from low-alloyed steels and can be used, for example, in pipe rolling production. Method for thermo-friction cutting with a disk saw heated to temperature of 1150–1250 °C from low-alloy steel rolled stock with diameter of 40–120 mm includes separation of heated steel pipe by disc saw for thermo-friction cutting from low-alloy steel, containing all-metal body with wedge-shaped cutting teeth located along contour, each of which has a front negative angle equal to −35 degrees, an angle between the side surfaces of the tooth equal to 70 degrees, a positive rear angle α, as well as side angle of saw tooth bevel ϕ. Heat-friction cutting of heated rolled pipe from low-alloy steel with diameter of 40 mm is carried out with a disk saw with sharpening angles of each tooth α and ϕ equal to 14 and 16 degrees, accordingly, for large diameters of cut steel pipes from the proposed range, the clearance angle is determined by the formula: α=α0-k⋅ΔD, and side angle of saw tooth ϕ - by formula: ϕ=ϕ0-k⋅ΔD, where α0 = 14 degrees, ϕ0 = 16 degrees, coefficient k = 0.05 degrees/mm, ΔD is an increase in the diameter of the cut pipe in mm compared to diameter of 40 mm, wherein saw feed makes 8–16 mcm/tooth and feed rate makes 0.06–0.13 m/s.
EFFECT: improvement of quality of surface of ends of workpieces after cutting and increase in durability of disk saws.
1 cl, 1 tbl, 2 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR THERMAL FRICTION CUTTING WITH A CIRCULAR SAW OF HEATED ROLLED PIPE WITH A DIAMETER OF 120-200 MM MADE OF LOW-ALLOY STEEL | 2021 |
|
RU2765008C1 |
METHOD FOR THERMO-FRICTION CUTTING OF HEATED ROLLED PIPE WITH DIAMETER OF 40-120 mm FROM LOW-CARBON STEEL WITH DISK SAW | 2021 |
|
RU2767363C1 |
METHOD FOR THERMO-FRICTION CUTTING OF HEATED ROLLED PIPE WITH DIAMETER OF 120-200 mm FROM LOW-CARBON STEEL WITH DISK SAW | 2021 |
|
RU2767366C1 |
METHOD FOR THERMAL FRICTION CUTTING OF HEATED PIPE WITH DIAMETER OF 120-200 mm FROM AUSTENITIC CHROMIUM-NICKEL STEEL WITH DISK SAW | 2021 |
|
RU2767354C1 |
METHOD FOR THERMO-FRICTION CUTTING WITH DISC SAW OF HEATED PIPE WITH DIAMETER OF 40-120 mm FROM AUSTENITIC CHROMIUM-NICKEL STEEL | 2021 |
|
RU2767341C1 |
METHOD FOR THERMAL FRICTION CUTTING OF HEATED PIPE WITH DIAMETER OF 120-200 mm FROM AUSTENITIC CHROMIUM-NICKEL STEEL WITH DISK SAW | 2021 |
|
RU2767358C1 |
METHOD FOR THERMO-FRICTION CUTTING OF HEATED ROLLED PIPE WITH DIAMETER OF 120-200 mm FROM LOW-ALLOY STEEL WITH DISK SAW | 2021 |
|
RU2767362C1 |
METHOD FOR THERMO-FRICTION CUTTING OF HEATED ROLLED PIPE WITH DIAMETER OF 120-200 mm FROM LOW-CARBON STEEL WITH DISK SAW | 2021 |
|
RU2767368C1 |
2020 |
|
RU2749964C1 | |
METHOD FOR THERMOFRICTIONAL CUTTING WITH CIRCULAR SAW OF HEATED PIPES MADE OF LOW-ALLOY STEEL WITH DIAMETER OF 120-140 mm | 2023 |
|
RU2811877C1 |
Authors
Dates
2022-03-17—Published
2021-03-26—Filed