FIELD: construction.
SUBSTANCE: invention relates to an expanding admixture for tensioning and expanding cements. The expanding additive includes blast-furnace granulated slag, gypsum stone and alumina slag, and additionally contains iron-containing pulverized waste with a particle size of 1-200 microns. To prepare the mixture, components with a moisture content of 1–5% are used.
EFFECT: invention improves the strength characteristics of cements.
2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
EXPANSION ADMIXTURE BASED ON IRON-CONTAINING PULVERIZED WASTE FOR EXPANDING CEMENT | 2021 |
|
RU2767481C1 |
COMPLEX EXPANDING ADDITIVE FOR SELF-COMPACTING CONCRETE MIXTURE | 2019 |
|
RU2724083C1 |
EXPANDING CEMENT MIX | 2001 |
|
RU2229449C2 |
FAST-HARDENING CONSTRUCTION COMPOUND BASED ON STEEL SLAG | 2017 |
|
RU2647010C1 |
METHOD OF BUILDING MATERIAL MAKING | 1991 |
|
RU2031875C1 |
SHRINKPROOF COMPOUND FOR CONCRETE MIX | 2021 |
|
RU2779157C1 |
CEMENT | 1994 |
|
RU2079458C1 |
COMPOSITE WATER-RESISTANT GYPSUM BINDING AGENT | 2012 |
|
RU2505504C1 |
EXPANDING ADDITION TO CEMENT | 1993 |
|
RU2049081C1 |
METHOD FOR STEELMAKING PROCESSING WASTE RECYCLING TO PRODUCE PORTLANDCEMENT CLINKER AND CAST IRON | 2016 |
|
RU2629424C1 |
Authors
Dates
2022-03-28—Published
2021-10-13—Filed