FIELD: chemical industry. SUBSTANCE: aluminium is subjected for electroerosion dispersing in water with carbon dioxide feeding to it. Carbon dioxide is added at the dose 0.3-1.6 kg per 1 kg dispersed aluminium, and products of erosion were boiled. Proposed method ensures to decrease the content of baierite and metal in aluminium hydroxide and carriers and catalysts can be made of its. EFFECT: enhanced purity of product. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF ALUMINIUM OXIDE | 1991 |
|
RU2038304C1 |
PROCESS FOR PREPARING METAL HYDROXOALUMINATES | 0 |
|
SU1816738A1 |
DEVICE FOR ELECTROEROSION DISPERSION OF FERROMAGNETIC MATERIALS | 1984 |
|
SU1246488A1 |
METHOD FOR PRODUCTION OF IRON OXIDE PIGMENT AND UNIT FOR ITS REALIZATION | 1992 |
|
RU2043303C1 |
METHOD OF PREPARING CATALYST FOR CLEANING HYDROCARBON GASES FROM SULFUR ORGANIC COMPOUNDS | 1989 |
|
RU1653221C |
METHOD OF PREPARING IRON-MOLIBDENUM CATALYST FOR OXIDIZING METHANOL TO FORMALDEHYDE | 0 |
|
SU1313500A1 |
METHOD OF PREPARING CATALYST FOR SECOND STAGE OF AMMONIUM OXIDATION | 1988 |
|
SU1541833A1 |
APPARATUS FOR ELECTRO-EROSION DISPERSING OF METALS | 0 |
|
SU1217581A1 |
METHOD OF PRODUCING POWDERS AND PASTES | 0 |
|
SU1025494A1 |
POWDER PRODUCTION UNIT | 1987 |
|
SU1445111A1 |
Authors
Dates
1995-05-20—Published
1987-07-13—Filed