FIELD: electrical equipment. SUBSTANCE: bimetallic cermet electric contact has working and auxiliary layers. Working layer of bimetallic cermet contact consists of composition: graphite 1-3.5 mas. the balance, silver. Auxiliary layer of bimetallic cermet contact consists of silver in the amount of 26-34 mas. the balance, copper. Introduction into auxiliary layer of silver in the amount of 26-34 mas. makes it possible to increase electrical endurance of contact. EFFECT: increased electrical endurance of contact. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METAL-CERAMIC BIMETAL ELECTRIC CONTACT | 1985 |
|
SU1313244A1 |
MIXTURE FOR PROCESS PRECOAT OF CERMET ELECTRIC CONTACTS | 1985 |
|
SU1355024A1 |
CONTAKT PAIR LOW-VOLTAGE ELEKTRIC APPARATUS | 1992 |
|
RU2037226C1 |
BIMETALLIC CERMET FOR ELECTRICAL CONTACTS | 1987 |
|
SU1487289A1 |
METAL-CERAMIC BIMETAL MATERIAL FOR ELECTRIC CONTACTS | 1984 |
|
SU1415970A1 |
MIXTURE FOR PROCESS PRECOAT OF CERMET SILVER-CONTAINING CONTACT | 1989 |
|
SU1605861A1 |
MIXTURE FOR PRECOAT OF POWDER SILVER-CONTAINING BIMETALLIC ELECTRIC CONTACTS | 1987 |
|
SU1471888A1 |
MATERIAL FOR ELECTRIC CONTACTS BASED ON COMPOSITION OF SILVER-LEAD OXIDE | 1993 |
|
RU2032954C1 |
BIMETAL METAL-CERAMIC MATERIAL FOR ELECTRIC CONTACTS | 1985 |
|
SU1272909A1 |
CHARGE PREPARING METHOD | 1988 |
|
SU1577173A1 |
Authors
Dates
1995-06-19—Published
1988-05-23—Filed